台化聚苯乙烯塑膠粒物性彙總表下载
TAIRIREX Polystyrene resin consolidated property data sheet
項 目
Property |
單 位
Unit |
試驗方法
Test Method |
試驗條件
Test Condition |
MP6500 |
抗張強度
Tensile Strength |
kg/cm2
( MPa) |
ASTM
D-638
( ISO527) |
23℃ |
270
(26) |
伸長率
Tensile Elongation |
% |
ASTM
D-638
( ISO527) |
23℃ |
40 |
彎曲強度
Flexural Strength |
kg/cm2
( MPa) |
ASTM
D-790
( ISO178) |
23℃ |
520
(51) |
彎曲模數
Flexural Modulus |
kg/cm2*104
( MPa) |
ASTM
D-790
( ISO178) |
23℃ |
2.5
(2452) |
Izod衝擊強度
Izod
Impact Strength |
kg-cm/cm
( J/m ) |
ASTM
D-256
( ISO R180 ) |
23℃
1/4'' 厚 |
6.5
(64) |
衛氏軟化點
Vicat Softening
Temperature |
℃ |
ASTM
D-1525
(ISO306B) |
Annealed
80℃×2Hr
1/8'' 厚 |
97 |
熱變形溫度
Heat Deflection
Temperature |
℃ |
ASTM
D-648
(ISO 75/A) |
Annealed
80℃×2Hr
1/8'' 厚 |
89 |
熔融指數
Melt
Flow Index |
g/10 min |
ASTM
D-1238
( ISO1133 ) |
200℃×5Kg
( 49N ) |
7.0 |
殘留單體
Residual Monomer |
ppm max. |
|
|
700 |
比 重
Specific Gravity |
|
ASTM
D-792
( ISO1183 ) |
23℃/23℃ |
1.04 |
燃燒性
Flammability |
|
UL-94 |
FILE NO.
E162823 |
1/16" HB
NC |
以上數值係依照ASTM試驗方法所測得,僅供選擇用途品級之參考。
|